Under the premise of ensuring the full melting of the ingredients in the high temperature area, the shorter the solemnity; the cooling speed has a great impact on the intensity of the joint. Generally, the time from 880 ° C to 200 ° C should be controlled after welding. Between 5 and 20 minutes; the fire -retitating temperature between 350 and 450 ° C has a trough area. Tripplailia welding uses HL105 ravioli, with appropriate tadpole to obtain the ideal connector performance.